Gold plating on silver zari, and alternatives




January 24, 2021
wikipedia
Zari (thread)

Q. I need to find an alternative for gold plating in running a process for zari manufacture. Someone help me out if you know any options are there.

Jay patel
- surat Gujarat




⇩ Closely related postings, oldest first ⇩



Q. How is silver zari (used in silk sari weaving for borders) gold plated? And could you provide a list of basic chemicals needed for making an immersion plating of gold on the metallic silk threads?

Umapathy
hobbyist - Chennai, Tamilnadu, India
2004



2004

A. You can use next solution:

7 gm gold chloride
30 gm potassium ferrocyanide [affil links]
30 gm potassium carbonate
30 gm sodium chloride
1 lit water,95 °C temp., objects must be in contact with zinc or aluminum!

Good luck!

Goran Budija
- Cerovski vrh Croatia




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"