Spec for Zi-Cu-Ni electroplating over Aluminum?





May 2, 2011

Hello everybody, I have a little problem in my facility, I'm searching for any spec that controls plating over Al, with Zi, Cu with electrical current and Ni with electrical current.

Does you know any spec for this?

Thank you in advance, regards.

Eduardo Castillo
Aerospace - Quer´taro, Mexico



June 14, 2011

Hi Eduardo,

You may refer to ASTM Standard B 253 - Standard Guide for
Preparation of Aluminum Alloys for Electroplating. A copy is available for purchase at www.astm.org/Standards/B253.htm

Regards,
David

David Shiu
David Shiu
- Singapore


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"