Nickel Plating for NiFe Batteries




I am experimenting with a design for NiFe batteries, and would like to know what kind of base material would/could be used to plate with nickel.

The plates are submersed in Potassium Hydroxide electrolyte.

A "Guess" on price would be very important. The cathode (Ni) would need to have a surface area of approximately 24 square inches.

Thanks for any response.

Dave

Dave Rowland
product designer - Summerdale, Alabama, USA
April 12, 2011


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"