Sodium Cyanide wrongly added to Potassium Cyanide based Silver Plating Solution




April 7, 2011

A plater by mistake has added 10 kg (22.4lb)of sodium cyanide instead of KCN to a potassium cyanide based silver plating solution. The operating limit of free KCN is
8 - 12 oz.wt/gal.
What will be the effect on the plating deposit quality, if used as it is and the KCN addition done in the future?

Kebede Jimma
Plating Shop Senior Supervisor - Abu Dhabi, UAE



You will not notice any problem

robert probert
Robert H Probert
Robert H Probert Technical Services
supporting advertiser
Garner, North Carolina
probertbanner
April 7, 2011



April 10, 2011

No harm done.
There are platers who use a combination of potassium and sodium cyanide for silver plating.

sara michaeli
sara michaeli signature
Sara Michaeli
Tel-Aviv-Yafo, Israel



Shouldn't be any problem

trevor crichton
Trevor Crichton
R&D practical scientist
Chesham, Bucks, UK
April 18, 2011


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"