-----Copper Oxidation
How to prevent oxidation of copper in cables specially in moisture conditions. So that the glare of copper wire should also increase?
Vikas Gulatidesigners - New Delhi, India
2000
You probably want to use a benzatriazole solution; these can be purchased from many suppliers.

James Totter, CEF
- Tallahassee, Florida
2000
Question how to prevent oxidation of copper in cables specially in moisture conditions. So that the glare of copper wire should also increase?
Peter Mongadicables - South Africa
2002