-----Painting on different automotive substrates (Stainless Steel & Aluminium)
Greetings
I would like to know which of the following is a bigger challenge as a process and why
- Painting on Stainless Steel sheets
- Painting on Aluminium sheets
I ask this question for my academic interest.
Thanking you with regards
Sony
Process Engineer - Bangalore, Karnataka, India
August 31, 2010
Hi, Sony.
In view of the fact that there are thousands upon thousands of acres of painted aluminum roofing and siding exposed to the elements, I'd have to say that stainless steel presents a bigger challenge 🙂
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
August 31, 2010
Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.