-----Powder coating changes color from heat and humidity
Dear Sir
After powder coating when the material is placed in the temperature of 50 degree and in the humidity of 95% then the colour of the material is changed.Give me some solution for that problem.
- Ecil, Hyderabad, AP, India
August 27, 2010
To obtain any help with your problem you need to inform the readers...
a) The metal substrate Al or Fe etc?
b) Type of coating used?
c) Pretreatment if any?
d) What test equipment is being used... if any?
e) What is the start colour and defect colour... an image may help?
Birmingham, United Kingdom
August 31, 2010
Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.