-----Cold dipped galvanizing process [Singapore]
I would like to know the process of cold dipped galvanizing (not the painting type) like what is the surface preparation, after surface preparation is it followed by fluxing, and then galvanizing. Is there a BS Standard for this process or coating?
Chua Sallycontractor for Architectural work - Singapore
July 22, 2010
July 22, 2010
Hi, Chua. Are you referring to zinc electroplating -- sometimes called electrogalvanizing?