Want antitarnish treatment for bright dipped brass that is good to 200 C




Brass items once Etched in Acid Dip gets rid of all oxide layer & get gold shine but shine do not remain stable, Suggest me good antitarnish which is stable at high temperature 200 °C.

Kalpana Charya
plating shop employee - Ranjangaon, Pune, India
March 2, 2010



April 25, 2010

GM,
Try using Benzotriazole [adv: item on eBay or Amazon] in the final hot water dip in preventing the tarnishing after bright dip.

All the best.

SHANKARANARAYANAN N
- Bangalore, KARNATAKA




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"