Is anodizing of galvanised sheet steel possible (PGI)

none
adv.
this text gets replaced with bannerText
spacer gets replaced with bannerImages



Acronyms:
PGI = pre-painted galvanized iron

Q. We are a company that manufactures acoustic louvres from either stainless or PGI. We have had a query from a customer who wants our acoustic louvres made in PGI anodized when finished (we usually powder coat). My question is can PGI be anodized? if YES what are the advantages to doing it? If NO why can't it be done.

Hamish Miller
manufacturer - Perth, Western Australia, Australia
November 6, 2008


SOME SUGGESTED GALVANIZING BOOKS
for Shops, Specifiers & Engineers


"Hot Dip Galvanizing of Steel Structures" by Kuklik & Kudlacek (2016)
avail from eBay, AbeBooks, or Amazon

"Handbook of Hot Dip Galvanization" by Maass & Peissker (2011)
avail from eBay, AbeBooks, or Amazon

"Galvanized Steel Reinforcement in Concrete" by Stephen Yeomans (2004)
avail from eBay, AbeBooks, or Amazon

"Hot Dip Galvanizing -- A Guide to Process Selection & Galvanizing Practice" by M. J. Hornsby (1995)
avail from eBay, AbeBooks, or Amazon

"Faults in Hot-Dip Galvanizing" by Dietrich Horstmann (in English, French & German)
avail from Amazon

"User's Guide to Hot Dip Galvanizing for Corrosion Protection in Atmospheric Service" by NACE (1997 only rarely avail.)
avail from AbeBooks, or Amazon

(as an Amazon Associate & eBay Partner, finishing.com earns from qualifying purchases)

A. Hi, Hamish. No, anodized galvanizing is not commercially available. It can't be done usefully & practically without an intense development effort, and maybe not even then :-(

Anodizing is a process where a component is wet processed and subjected to anodic current to convert the metal on the surface to an oxide. Depending on the metal, this may form a tight, adherent, corrosion-resistant surface, and it is done gainfully on aluminum, titanium, and magnesium. But for some other metals the process is useless; steel for example cannot be usefully anodized because its oxide, rust, is a loose, powdery, hygroscopic material which does not slow further rusting.

Solid zinc can be anodized and the corrosion resistance is excellent, but it requires very high voltages, and is rather impractical for other reasons, and the process never found commercial favor. So could you usefully anodize the galvanized skin without exposing the steel? In a lab maybe. But I think you are very far from being able to offer it commercially (not that I would discourage the research if you have the resources). But a customer specifying anodized galvanizing is almost surely just making a mistake, and is not specifying a commercially available finish :-)

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




Multiple threads were merged: please forgive repetition, chronology errors, or disrespect towards other postings [they weren't on the same page] :-)



Q. I'm trying to bid on a job that identifies the material as 1 1/2 inch diameter galvanized in the plan view and dark bronze anodized in the elevation view. This is a state job and I missed the cut off time for questions by one day.

Dale Aliano
Welding fabricator - Salinas, California, United States
August 28, 2009


A. Hi, Dale. There is a very rarely used and non-commercialized process for anodizing zinc; theoretically speaking, it might be possible to anodize the galvanized coating, but . . .

Speaking more practically, either there is an error on the drawing or you are misreading it.

Luck & Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"