finishing.com -- The Home Page of the Finishing Industry Search our quarter-million Q&As

Home of the finishing HOTLINE since 1989

-----

Weatherizing new copper to match existing panels




Hi, I have a company that has an airconditioning unit on the roof of their building. Some hoodlum stole two sheets. The insurance company has asked us to replace the sheets but with the 2 new sheets put up against the old sheets it will not look nice. What can I use to pre-weather the copper to match the old copper?

Angie Larue
remodeling contractor - Bristol, Connecticut
August 8, 2008



Hi, Angie. When in the third world, do what the third worlders do. You won't get a good match and the hoodlums will steal a mix of new and old next week anyway. So beat them to it by selling the remaining copper for scrap yourself, then replace it all with copper colored aluminum :-)

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
August 11, 2008


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"