Copper plating


(2000)

I would like to know if I can plate die cast or pot metal with electroless copper. Can I do this or must I use electro plating or cyanide? Any help is greatly appreciated. Thank you very much.

Mark Robidoux
- malvern


(2000)

To my knowledge, you can't beneficially apply electroless copper to die cast or pot metal, and must use cyanide copper electroplating (or possibly copper pyrophosphate) but please give us more specifics about your company's aim here so that we don't have to limit our answer to a yes or no. Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.