Black oxidizer on aluminium


(2000)

Luc Paquet

I want to make a black finish on aluminium surgical tools.

I want a dark black color with non-conductivity, and a good resistance to cleaning and sterilization procedure.

I'll waiting for a answer.

merci! Luc.

LUC PAQUET
Atelier Soluc inc. - Quebec, Canada


(2000)

What types of cleaners and sterilizing chemicals do you use? A black oxide would be black, that part is true, but it would still be conductive, as it is nothing more than a conversion coating process. The other option that I could think of would of course be black anodizing, which solves both the issues you have as far as color and I'm assuming it would stand up the sterilization process, but again, knowing exactly what the things used to clean the tool(s) would be helpful. If this doesn't work, maybe someone out there could do a black nickel on aluminum (is it possible? Anyone able to do this process to confirm for me?)

Matthew Stiltner
J & J Plating Company - Toledo, Ohio



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.