Verdigris - zinc


(2000)

Can anyone tell me how I can speed up the process of verdigris on zinc to achieve the green patina one sees on aged zinc clad rooftops. Best regards James Fox

james Fox
- london england


(2000)

James, unfortunately it's gonna take until pigs fly. Verdigris green patina occurs on copper roofs, not on zinc ones, because the green color is a copper salt. Zinc roofs just eventually rust when the galvanizing wears off. Sorry.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.