Looking for Permalloy Electroplating Service



I'm a graduate student researcher of the Department of Electrical and Computer Engineering, University of California, Irvine. I'm currently working on a MEMS project to fabricate a microactuator.

I need some help with respect to the plating of permalloy. If someone knows which organization has the facility for permalloy plating, please kindly advise. A facility around Los Angeles area is preferred.

Thanks so much!

Jun Hua
UC Irvine - Irvine, California, USA


Sorry, I don't know a shop in California, but Materials Innovation, 8 Commerce Ave., West Lebanon, New Hampshire is a good bet for high-tech low-volume permalloy plating.

Ted Mooney, Teds signature
Ted Mooney, P.E.
Pine Beach, New Jersey


Hi, Does anybody have the expertise on how to electroplating copper onto permalloy? I would like to consult you. Thanks so much! Jun Hua UC Irvine

Jun Hua
UC Irvine - Irvine, California, USA


Snagged again, for the thousandth timesmiley.

I thought that by 'permalloy electroplating' he meant electroplating OF permalloy onto something else; but he meant electroplating of something else ONTO permalloy.

Ted Mooney,
Teds signature
Ted Mooney, P.E.
Pine Beach, New Jersey


Thanks so much Ted. What I actually need is, first, electroplating a permalloy thin film onto silicon substrate; second, etch away the undesired portion of the permalloy; third, electroplating copper onto the permalloy layer; forth, etch the copper layer to form a pattern.

I'm still wondering where to find the whole process.

Jun Hua
UC Irvine - Irvine, California, USA


I have found UHV Sputtering of San Jose to be a reliable supplier of electronic grade thin films of permalloy on silicon wafers.

Robert Ditizio
Tegal Corporation - Petaluma, California, USA

This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site


Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices

©1995-2018, Inc., Pine Beach, NJ   -   About   -  Privacy Policy
How Google uses data when you visit this site.