I am trying to start a small mail order magic shop. One of the items I wish to sell involves a small shiny plastic ball. I am looking for a inexpensive way to chrome plate them. They are about 3" in diameter with a small hole of about 3/4". I will only need about a dozen plated to start with. I will be grateful for any help in getting these plated. Thanks Dale Burden

Dale Burden
- Owensboro, Kentucky USA


(2000)

Unfortunately, this is not an easy one.

Actual nickel-chrome electroplating on plastic, such as is done on automobile grills and bezels can only be done on certain special grades of plastic. Vacuum metallizing (depositing a shiny aluminum film followed by a thin lacquer) sounds more applicable to your needs but I don't know if you'll find a shop to run such a small order through such expensive equipment. Shops you might talk to include Associated Electroplaters [Hazel Park, Michigan], Cybershield International [Dallas, Texas], Providence Metallizing [Pawtucket, Rhode Island], and Quaker Precision Coating [Johnston, Rhode Island]



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.