Plating silica


(2000)

I am looking for a process of plating silica with Fe Co in a a sulfate bath. or if there is any methods for plating silica thanks

Jonathan Hughes
Boeing - Seattle, WA USA


(2000)

I assume you are looking for a metal plating/coating on silica (quartz). We have developed a PVD process for bonding metals directly to glass and ceramics, and then continuing to grow relatively thick coatings (> 10 micron). May be our process will work for you.

Mandar Sunthankar
- Fort Collins, Colorado



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.