Electropolishing 440C Stainless


(2000)

We're having trouble finding someone to electropolish some 440C Stainless parts... the fellow who'd done it for us in the past no longer works for that company... Help!

Thank you

Brian Lentz
Xandex - Petaluma CA USA


(2000)

Our company successfully electropolishes SS 440C. The process provides smoothness, cleanliness and passivity, with a low luster (not as bright as with some of the other stainless alloys). Samples for evaluation can be run at no charge.

Mary Wilk
Electromatic, Inc. - 789 South Kellogg Avenue, Goleta, California



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.