Post treatment coating for Salt Bath Nitriding


(2000)

Q. Hello, I'm a design engineer working on implementing Salt Bath Nitriding into some of our Zinc plating applications.

I need to know what are some of the post treatment coatings that can be applied? The nitriding process leaves surface porosity.

I have been told about Rust Veto, but are there others?

Thanks

Elizabeth A. Neumane
- Orlando, Florida, USA


A. Hi Elizabeth. Have you investigated Kolene's Quench-Polish-Quench process whereby (as I understand it) an intermediate polishing step removes the porosity?

Ted Mooney, finishing.com
Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey


September 15, 2014 -- this entry appended to this thread by editor in lieu of spawning a duplicative thread

Q. Hello sir. Give me a some idea for post oxidation process in liquid nitriding process, and tell me how to make this bath.
Please give me a reply.

Jaydeep Gosai
heat engineering works - Surat,Gujarat,India



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.