POWDER COATING: LOOKING FOR A FLUIDIZED BED COATING SYSTEM


(2000)

We are a dry-clean hangers manufacturer. I am looking for a FLUIDIZED DIP TANK (electrostatic) that will allow me to do powder coating on the wire hangers. Something cheap and simple. Not interested in spraying.

Thanks.

Gene

Gene Chu
Wells Mfg. - S. El Monte, Calif.


(2001)

Hello,

I am producing small metallic pieces (about 1 gr/un) I need to coat them using polyester powder coating, and the best way to do it is by the fluidized bed coating system. Can you tell me where to find this kind of machines?.

Thanks,

Luis Salazar
Fundiformas - Medellin, Antioquia, Colombia



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.