Hard Anodizing


(2000)

We are looking into coating an aluminum extrusion with a hard anodized coating to use as the track base for a linear slide. The linear slide rolls with 52100 steel guide wheels that will ride directly on the coated aluminum surface. Loads will be relatively light. Is there a coating or a process that will work with a minimal amount of wear? or are the steel guide wheels too much for any coating? The slides may be lubricated.

Thanks

Jeff Mitchell
Pleasant Hill, California


(2000)

We have a chromium nitride coating that we've been able to deposit on aluminum alloys without mechanical degradation. The hardness of the coating is around 2100 Hk, and the adhesion is outstanding. We'd be happy to look at coating the rails for you.

jim treglio portrait
Jim Treglio
- Vista, California


(2000)

Dear Sir,

We are in the field of colour & hard anodising. I would like to request you to help me out in carrying out grey colour hard anodising for aluminium machine parts. Kindly also let me know various types of buffing for getting quality finish. waiting for your reply. Kindly also let me know if I can get any brochures for hard anodising. With regards Taher

Mr. Taher H.Chiniwala
M/s. Chiniwalas Pvt. ltd. - Pune, Maharashtra, India



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.