Need Help to achieve aged white paint effect on decorative cast Iron.


(2000)

Dear Sirs,

We have a project where we need to achieve an aged paint effect in white on cast iron decorative urns, etc. I'm working with a rust base and for this item we are not too concerned about more natural rust occurring.

The materials we need to use need to be found easily in China. Most preferred solution would be something we could place on the paint after it's applied to age and breakdown the paint, hopefully causing cracking and flaking.

If you can be of any assistance that would be greatly appreciated.

Regards,

John Muldoon
- Shanghai, China



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.