(2000)

I am trying to age T2 tinplate from the factory shine to a darker pewter-like colour. I have soaked the panels in 5% acetic acid ( vinegar ) but this doesn't seem to work. Any ideas? Thanks.

Joe O'Donohoe
- Ontario,Canada

(2001)

I have had customers who use a two step process of caustic - then rinse - then use "gun barrel bluing"

Michael Amann
- Baltimore, Maryland, USA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.