I am looking for a process known as Magnesium Dichromate. I am in the Racecar business and all the Mag parts are treated this way. I would like to start doing this in house being that the parts get abused. The treatment is Black in color and is very thin. Any help would be greatly appreciated.

Thank you,

Jason Weissman
CDI MotorSports - Morris Plains New Jersey, USA


(2000)

I would not recommend setting this up at home.

David A. Kraft
- Long Island City, New York


(2000)

I would agree about not doing it at home, but "in house" does not necessarily mean at home. Boeing does a lot of chemical processing "in house" smiley

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.