Identify Metal Finish Zactique


(2000)

We are trying to gather information on a metal finish we believe to be called " zactique ". That may not be the proper way to spell it, we were given the name verbally over the phone by a client who wasn't sure of the correct spelling either. In any case all information on this finish as well as who has it would be appreciated.

Respectfully submitted,

Mark VanDenHam
- Chatsworth, California


(2000)

Mark, Much slang is encountered in the metal finishing industry. Find out what object (objects) your client is wanting to have electroplated or the resulting finish. Is it "indoor or outdoor" for the items? Repost your question again.

Bill Hemp
tech svc. w/ chemical supplier - Grand Rapids, Michigan


(2001)

I know that there is a coating made by IMSA that has this name. It is a metallic antique finish.

Corey Wallace
- Hamilton, Ontario, Canada



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.