Summary for ral munsell color conversion Discussion
RAL/Munsell color conversion is the main issue in this thread, with several readers asking for exact cross-matches such as RAL to Munsell and Munsell to RAL for specific shades. The replies stress that RAL and Munsell are different color standards, so there is no exact one-to-one conversion; at best, you can find the closest match. Rasawulan suggests using Munsell conversion resources and then a matching tool such as EasyRGB to identify the nearest RAL code, though the cited GretagMacbeth site is now noted as no longer functional. In a June 2023 editor’s note, the archive explains that it no longer makes sense to publish individual conversion requests because there are too many possible combinations and essentially no one answers them. The practical guidance is to use general conversion resources and accept approximate matches rather than exact equivalents.
Q. I am looking for a conversion chart or software for RAL to Munsell.
Jeff B. Thompson
– Mayfield, Kentucky
2000
Q. I would like to know conversion from Munsell 2.5 Y 8/4 to RAL code. Thanks for help.
Araldo Alexandre Silva
– Joinville, SC, Brazil
2000
A. Actually RAL and Munsell are using different standard of colors. So not exactly the same color for both. But you can find the closest one. You can use Munsell Conversion color from www.gretagmacbeth.com then go to www.easyrgb.com/matching.php3 to find the closest RAL Code.
Rasawulan
– Indonesia
Ed. note June 2023: www.gretagmacbeth.com appears to no longer be functional; www.easyrgb.com is functional, but not the specific page which Rasawulan referenced.
“Pantone: The Twentieth Century in Color”
by Eiseman & Recker
<!–
–>
<!–
on eBay
–>
or
or
or
(affil link)
Q. I would like to know conversion from RAL 5015 and RAL 7032 to Munsell code. Thanks for help (It’s urgent, so please inform us the answer)
Hwang, Joungsung
– Seoul, So. Korea
2001
Q. I would like to know conversion from green Munsell 2.5 4/8 to RAL code. Thanks for help
JOSE FUENTES
– Colchester, Essex, UK
2002
Q. I’m looking for Munsell to RAL color conversion for next values : Munsell 10GY 4/7, 7.5R4/14, 2.5YR6/13, 2.5YR6/18, 2.5YR3.5/3.5,
2.5P5/5, 2.5G3/5, 2.5Y8/2, 5B8/4, 10B5/10, 2.5PB3.5/10, 2.5G7/2
Alexandre Le Grelle
– Antwerp, Belgium
Q. I need Munsell n5.5 color equivalent to RAL code
Veeramani
– Chennai, India
Q.
I would like to know Ral# for Munsell code Green 10 GY 6/6
Lawrence Gatt
Coatings Supervisor – Lawrence, Scotland
May 29, 2023
Ed. note: Anyone is welcome to work these conversions and answer you, but unfortunately, time has demonstrated that no one will, so it’s impractical to post individual conversion requests between RAL, RGB, Munsell, Pantone, and CXF values or other color systems … At one point we received 5 such requests for posting in 48 hours and there are a virtually infinite number of such conversions! We’ve provided a FAQ on the topic with general guidance on how to go about it, and a list of resources, but with countless people wanting a specific conversion, and zero people willing to offer it, it no longer makes sense to publish requests for specific conversions. Thanks for your understanding.