Aloha, fun & authoritative answers -- no cost, no registration, no passwords, no popups
(as an eBay Partner & Amazon Affiliate we earn from qualifying purchases)

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
pub  Where the
world gathers for metal finishing
Q&As since 1989



-----

Cost to open a hot dip galvanizing business?

none
adv.
this text gets replaced with bannerText
spacer gets replaced with bannerImages


Q. I am a private person from North Macedonia, I am interested to start a new galvanizing plant here.
Is it possible to provide me any idea or any plan about investing budget and what is building time up to start working.

Faruk Aliu
- Tetovo, North Macedonia
February 15, 2024


A. Hi Faruk
For a first-cut very rough estimate, Geoff Crowley, Thomas Cook, and John Malone have already given you their guesses.

If you know how big a kettle you want, or how much work will be processed, etc., a closer guess might be forthcoming.

Luck & Regards,

pic of Ted Mooney
Ted Mooney, P.E. RET
Striving to live Aloha
finishing.com - Pine Beach, New Jersey


A. The question is not well enough defined to be able to give any meaningful answer.
It is like asking. "I want to purchase a vehicle, what will it cost?"

You will need to consider the market available, and from that assess the size of the plant, the level of automation, the amount of customisation for local materials costs, energy sources, etc.
Time to build could vary from 3 months to 3 years depending on these factors.
Cost could vary from USD 1m to 50m, depending on these factors.

geoff_crowley
Geoff Crowley
Crithwood Ltd.
supporting advertiser
Bathgate, Scotland, UK
crithwood logo







⇩ Closely related postings, oldest first ⇩



Q. Dear readers,

I will appreciate if somebody could advise me the equipments that are are required to start a small hot dipped galvanization plant. Or advice me where I can get some literature with respect to above.

We are in need of small hot dip galvanising plant to galvanise bolts & nuts, overhead electrical line hardware, etc..

Regards,

Yusufali
- Dar es Salaam, Tanzania
2002

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)




"Handbook of Hot Dip Galvanization"
by Maass & Peissker

on AbeBooks

or eBay or

Amazon

(affil links)

A. Hi, Yusufali. We've linked to a few good galvanizing books here, but it's an awfully broad subject, and you may be interested in talking to a supplier of galvanizing equipment or a galvanizing consultant to get you started. Good luck with it!

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




Please Quote on this Galvanizing Plant

User's Guide to Hot Dip Galvanizing for Corrosion Protection in Atmospheric Service
by NACE
[only rarely available]

on AbeBooks

or eBay or

Amazon

(affil links)

RFQ: Background:
Our firm, one of the biggest engineering industries in Ethiopia has been engaged in the manufacturing of engineering products for over twelve years now. The company, up to the present, has been involved in the production of the following engineering products.

· Manufacturing of cargo and tanker bodies
· Manufacturing of trailers and semi-trailers
· Assembly of cargo and dump trucks
· Fabrication of components and assembly of crushers
· Mega rolling and big size tanks and silos
· Electro-mechanical works
· Machining services

To undertake the above activities, the company has invested in the required machineries for steel construction, manufacturing, assembly, and electro-mechanical works, surface treatment, apart from the assembly lines for cargo and tanker bodies, trucks and crusher as well as a mega rolling plant for the manufacturing of tanks. The workshop is further supported with design and material and products testing facilities. We manufacture various equipment and components for the industrial, transport, construction, agriculture and other sectors. The industrial complex lies-over 250,000m2 premises 35,000m2 of which is covered area. Currently, it employs more than 450 workers

With an aim to be competitive for the local market and export market we decided to own Hot Dip Galvanization Plant as per the following specification

Specification of our requirements:
The plant shall have the following:

Surface preparation
Prefluxing
Galvanizing
Finishing

We would like to galvanize according to the specification and practices contained in ASTM standards --
ASTM A123,
ASTM A143,
ASTM A153 ,
ASTM A384,
ASTM A385,
ASTM A780

CAPACITY:
As Option 1, with 5000 ton/ two shift/year (16 hours/day)
Option 2, with 10,000ton/two shift/year ( 16 hours/day)
Option 3, with 15,000ton/two shift/year (16 hrs/day)
Maximum length of product to be galvanized: 7000 mm

Heating system shall be with furnace oil Local environmental demands exhaust system for zinc vapor from kettle and acid vapor from pickling, and waste disposal such as waste acid and iron sludge The plant shall have a future for future expansion to increase out put of the plant by 25-50% Training and know-how transfer Erection and commissioning please include required consumables to run the plant for a period of three months.

Our plan for implementation is to commission and erect the plant before February 2005. Based on the above, please send us your best proposal. Looking forward to your reply, I remain

Getachew Okbay
steel fabrication - Ethiopia
2004

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)






Need hot dip galvanized plant for Nut Bolt industry

RFQ: We are planning to Purchase a new hot dip galvanized plant for our Nut Bolt industry, with 500 Kg to 1 Ton Capacity /day. we would be be pleased to receive the Offers from the manufacturers at an earliest.

Please also dispatch the catalogues/Brochures for our Quality Evaluation and Future reference.

Thanking you and meantime looking forward to your further favors as requested to initiate with you a long lasting mutually beneficial business relations in the near future.

Thanks and best regards.

truly yours,

MAQSOOD SHAHAB, CHIEF EXECUTIVE
M/S Shahab Marketing Syndicate - GUJRANWALA., Punjab, PAKISTAN
2004

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)






Want to set up hot dip galvanizing plant

Q. We are planning to set up hot dip galvanizing plant in India.now we are doing feasibility studies. Could you send Techno economic report for setting up hot dip galvanizing plant in India?

Abdul Hadhi
- India
2006




How to start a new galvanising plant?

"Hot Dip Galvanizing
A Guide to process Selection & Galvanizing Practice"
by M. J. Hornsby

on AbeBooks

or eBay or

Amazon

(affil links)

Q. I want to start my own plant. Can you give information how and where to start? What do I need. I have about 112 m2 available.

Mr Stiaan Duvenage
Industrial - Hermanus, Western Cape, R.S.A.
2007


simultaneous replies

A. I'd suggest contacting one of these organisations as it's not possible to give the detailed information you require in a forum like this.

www.hdgasa.org.za/ (hot dip galvanizers association of South Africa)
www.galvanizersassociation.com (USA)
www.hdg.org.uk (UK)

John Martin
- Wales


A. This question is too vague to be answered here. It would take a book! Don't think this is the right forum for that question.

112 m2 available for what? That seems too small for even a model of a plant.

geoff_crowley
Geoff Crowley
Crithwood Ltd.
Westfield, Scotland, UK
crithwood logo


A. Hello Stiaan. I suspect that you surely must mean 112 m x 112 m :-)

That should be enough.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




Multiple threads were merged: please forgive repetition, chronology errors, or disrespect towards other postings [they weren't on the same page] :-)



Cost to open a hot dip galvanizing business?

Q. Hi Everybody
I would like to open a small hot dip galvanizing shop in North America. How much start up money do I need in order to have something competitive and contemporary? What are the factors and or any restrictions to keep in mind? Please advise!
Thank You

Anton Perjaklu
investor - Canada
July 12, 2008


A. This question is easier to answer ...

"I'd like to buy a car. How much will it cost?"

What sort? What size? Where? What quality? What energy supply? etc, etc.

But risking being argued off the page for making a huge number of assumptions, $CAN 8 million.

geoff_crowley
Geoff Crowley
Crithwood Ltd.
Westfield, Scotland, UK
crithwood logo


A. Sir,
About 10 to 20 years ago I estimated that a galvanizing plant costs about $100,000/foot of kettle length. Thus a 40 foot long kettle (the entire plant) would cost about $4,000,000. With inflation this is likely to be about $8,000,000+ today. Also kettles and all tanks are much deeper now than 10 to 20 years ago so $8,000,000 plus $2,000,000 = $10,000,000 may be more realistic. Actually far more important is the available market in the area that you would build. Thus I have estimated that you need about 1,000,000 pounds of steel for every foot of kettle length to make a decent profit. Thus for a 40 foot kettle you need at least 40,000,000 pounds of steel each year. There are a few places in the world where prices for galvanizing are high (islands, and high steel transport prices where a smaller amount of product could give a profit).

Regards,

Dr. Thomas H. Cook
Galvanizing Consultant - Hot Springs, South Dakota, USA


A. Based on almost 50 years of experience I would estimate the cost of constructing a new energy efficient (and environmentally friendly) hot dip galvanizing plant is $190,000 to $220,000 USD per LF of kettle ... PLUS cost of land, startup chemicals, and zinc.

John Malone
- Whitsett, North Carolina, USA
March 6, 2012




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software