| Search our quarter-million Q&As |
Home of the finishing HOTLINE since 1989
-----Wrought iron acid wash
Has anyone had any experience with acid washing wrought iron. What type of product is used to get this type of finish? Thank You
Jamie Kepler- Los Barriles, B.C.S., Mexico
2006
Most steel mills use hydrochloric (acido muriatico) acid to descale or "clean" their products. I don't know if that's the kind of finish that you are looking for.
Guillermo MarrufoMonterrey, NL, Mexico