Chrome wheels damaged by HCl





An apprentice at my company accidentally washed my wire chrome wheels on my classic sports car with Hydrochloric acid (we use this acid to remove concrete from construction plant) It appears to have removed the chrome plating but only in certain areas. Does any one have any ideas as to how I can re-polish the wheel without completely re-chroming it.

Thanks,

David Aldridge
Civil Engineering - London, United Kingdom
2006



Unfortunately that won't prove possible, David.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2006


adv.
M and M Metallizing banner

Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"