Sealing of colour after anodising


(2000)

We are engaged in the manufacturing of heat sinks in Aluminium extrusions.We have to anodise them and sometime colour them black as per our customer requirement. For black anodising the process we follow is

Even after following this process we have a problem of colour bleeding in IPA(Isopropyl Alcohol [linked by editor to product info at Amazon]).Please suggest foolproof method for sealing.

anil
sark ind. - india


(2000)

ANIL,

to overcome the problem of black dye bleeding out during sealing you should set up a two stage sealing process, the first containing a SEALING SALTS AS and the second containing ALBACLIN. Both these products are available from a company called CLARIANT. I have used both these products and have got very good results when when using black dyes.

david murphy
- Birmingham England



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.