(2000)

I am a retired person who works part time as an airsmith at a paintball field. In looking at a second career, I believe I would like to set up a business to anodize paintball guns with splash coatings and graphics. Where could information on learning to anodize this type of metal be found and approximately how much would it cost to equip a shop to do this type of work.

Doyle Dwight Crum
Crum & Son - Marietta, Georgia

(2000)

Doing any anodizing at all involves you in a rather substantial business, involving many vats of toxic chemicals, and the need for EPA licensing of your waste water and manifested wastes for landfill. To add splash anodizing, which involves some closely held trade secrets, increases the scope of the project. In other words, it's not going to be a part-time job, and if you plan it to be, you will be miserable rather than happy. I'd suggest getting a couple of our "must have" books and, after leafing through them, seeing if the prospect still interests you.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.