Counterflow Rinsing Help


(2000)

I am looking for info to help design a counterflow system for our rinse tanks. Any help greatly appreciated.

David A. Kraft
- Long Island City, New York


(2000)

The first stop is Ted's 20 ways to save water.

There are literally hundreds of constraints or factors in your question and you have given zero information. a very few are:

This is not rocket science or brain surgery, but experience in affordable retrofit is very beneficial.

You probably need a consultant. I am very inexpensive but require complete information to provide a quality service. Consider a good consultant, hands on type, that is in your local area.

James Watts
- Navarre, Florida


(2000)

David: I have limited experience in designing overflow / counterflow systems for rinse tanks. Please advise your tank specifications, and we'll try to reach you to provide you with some guidance.

Richard Toms
- Macon, Georgia


(2000)

Hello David,

My suggestion to you would be to check out Poly Products EV-II/III evaporator systems.

Matthew Stiltner
plating company - Toledo, Ohio



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.