Info on commercial gold bath companies


(2000)

I'm trying to electroplate gold as part of my research. I've tried several baths from acidic to alkaline, all of which contained Potassium Gold Cyanide. I'm looking for a deposit with low resistivity and a smooth surface, which has microstructure implications as well as substrate roughness implications.

Realizing there are some additives and operating conditions already worked out for this type of deposit, I've decided I'd like to try some commercial non-cyanide baths to avoid reinventing the wheel. I've seen Technic promoted here several times for gold plating needs. I've contacted them but I would like a couple of choices if possible. Does anyone recommend any other companies for gold plating baths? Has anyone heard of OMI Sel-Rex? They were recommended by my sponsor, without an address or contact. I cannot find OMI Sel-Rex in the Thomas Register or anywhere on the web. Any help would be appreciated.

John Florkey
- Columbus, Ohio


(2000)

Sel-Rex was bought out by OMI many years ago. More recently OMI merged with Enthone to become Enthone-OMI. They are in New Haven, CT.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey


(2000)

Shipley Ronal in Freeport, NY is another gold plating bath supplier.


Jerry Smith
- Paterson, NJ USA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.