How do you sulfuric anodize?


(2000)

I need requirements for sulfuric acid anodizing, times, temps, concentrations, soft and hard for aluminum, any information would be appreciated

Steve Adams
Metalcraft technologies - cedar city


(2000)

There is so much more to it than just the sulfuric acid anodizing tank itself that I think you may be misled if your questions are simply answered. First there is the issue of alloy and whether the item is wrought or cast; some anodize well, some poorly, and some almost not at all. Then the mechanical prep. Then the non-etch cleaner, the etch process, and the desmut before the anodizing. After anodizing is the rinsing, perhaps including bicarbonate neutralization or dilute nitric wetting, then the dyeing, the sealing, and the final rinsing.

letters #946 and #1148 will answer most of your questions about the sulfuric acid anodizing step proper.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.