Help with Zinc Cobalt on 380 Aluminum Die Cast components


(2000)

We are having difficulty consistently plating 380 Aluminum Die Cast components with Zinc Cobalt. Any suggestions or direction for process lines?

Don McClintock
- Paso Robles, California


(2000)

Dear Mr Don.

A process that works for us is to first Double Zincate, Copper flash, Cobalt Zinc plate and passivate.

If you want to avoid the cyanide copper flash try normal Acid Zinc plating for a few minutes then go to cobalt zinc.

Regards,

Khozem Vahaanwala
Khozem Vahaanwala
Saify Ind supporting advertiser
Bangalore, Karnataka, India

saify logo



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.