Looking for heat resistant powder and pretreatment process for the same.


(2000)

sirs/mam, hi I am into powder coating business. we are job coaters of automobile industries. what information I want or rather need is as follows:

1. is there any company that manufactures high heat/thermal resistant powder.(400-700 deg C).

2. the process or pretreatment needed to do for withstanding such high temp.

3. the base metal is made of CRC DD quality thickness 0.8 mm. please people this is an urgent help I need from anyone who knows abt this information.

thanking u

manoj s [last name deleted for privacy by Editor]
- aurangabad,Maharashtra,India

----
Ed. note: Readers, please restrict public discussion to the technical aspects of the question. Our experience indicates that public brand-to-brand comparisons rarely work out well considering the anonymity of the internet and the impracticality of determining the vested interests of the responders, so we don't print them. Thanks for your understanding.


(2000)

I've done some testing of powder paints applied to an aluminized steel substrate, tested up to 485 °C, as we've considered switching to powder on two occasions.

David Marion
- Winnipeg, MB, Canada



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.