My employer is thinking about offering Aluminum Flame Spray as one of our operations. Since I handle the environmental side of things, I'm looking for as much information as possible about the procedure. As this is only in the discussion stage, I don't have all the incidentals. Still, would one of you please be so kind as to point me to either a good web site or perhaps a book that could answer some of my questions? For instance, the regulatory limits, how possibly to classify the waste, safety issues connected to this process, etc. I appreciate any and all help. Thanks.

Kathleen Ferraz
- Austin, Texas


(2002)

I've worked with thermo coating , BOC Edwards Kachina and Pentagon in the last 6 years. They all offer aluminum flamespray. Are you still thinking of getting into flamespray or have you already gotten it?

Frank Guzman
- Austin, Texas



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.