I am doing research for a children's magazine. The article I am writing concerns metallic content of various coins past and present.

I have observed an interesting phenomenon. If quarters are left in water with pennies, all 1999 quarters turn blue. All quarters minted prior to 1999 do not. The U.S. Mint claims that the materials haven't changed. Allegedly, the current quarters still contain the same percentage of metals, 8.33% nickel, the balance copper.

Should I believe the U.S. Mint?

Does anyone have an explanation for the blue quarters?

Thomas J. Barstow
- Great Barrington, Massachusetts


(2000)

An experiment is worth a thousand guesses/opinions, so believe your results. However, a variable that you may not be taking into account is oils and tarnish on the older quarters that may be impeding the reaction. Scrub the old ones with a toothbrush and vinegar and salt, foul the new ones with butter or bacon grease, then put them all through the same cleaning regimen.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.