| Search our quarter-million Q&As |
Home of the finishing HOTLINE since 1989
-----Alternatives to zinc plated BBQ grills
2006
I would like to know if Zinc Plated items such as Grilling and Roasting Racks are safe for use on BBQ's
If Not, apart from Stainless Steel what would be the best plating to use for such BBQ racks and Utensils
Regards,
trading - Brunswick, Victoria, Australia
I'd say they should be nickel plated. Not so much as a matter of safety but as a matter of durability. BBQs are hot enough to vaporize the zinc. Alternately, ceramic coated.

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
2006
I suggest to plate with electroless nickel
alfonso meza- san jose California
February 16, 2010
Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.