Impact of lead anode lug contact on bus bar, if we increase the width of lug will it help to get better contact, will it help to increase the liberator efficiency for copper extraction.
Pradeep Mathew
2006
2006
Hello, Pradeep. If you have a highway that alternates between two lanes and three lanes, it will help traffic a great deal if you add a lane to the 2-lane area, but help little if you add a lane to the
3-lane area. We don't have enough information to know for sure whether the area where you are widening the current path is similar to the 2-lane area or the 3-lane area. However, since the conductivity of lead is very much less than copper, I suspect that you are probably on the right path.

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
If we frame lead anode with copper will it help for getting better result in liberator efficiency.
Pradeep Mathew
2006