topic 4107

HARD ANODISING COLOUR


(1999)

Dear sir,

We are facing the following problems in our Hard coat Anodising. Patchy marks like small round, found after hard anodising. In these areas colour is dull, and we tried with regular cleaning methods only. please advise us how to avoid this, can we do any special pre cleaning process or this is a raw material problem.

ELANGOVAN
- INDIA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.