Powder coating polycarbonate and its process


(1999)

I am looking for info on powder coating plastics. Is there a low cure powder out there that will work on polycarbonate. If so what would the process require? I presently manage a plastic painting operation and would like to take it to the next level. Any info would be greatly appreciated.

THANK YOU
Randy S.

Randy Schroeder
- Easley, South Carolina


(1999)

Powder coating on plastics and such is not uncommon. I have a client who is powder coating fiberglass braces with polycarbonate inlay. There are many low cure (200-220 deg. F) powders out there today but high gloss is still a problem - for most.

The first determination is the temperature your substrate can withstand before causing problems. After that is taken care of we can find the right powder and process for your application. Contact Morton powder coating and Forest Paints (Eugene Or.) for more information on low cure powder coats.

Joe Smith
- Portland, Oregon



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.