Student science project: the process of gold plating


(1999)

hi! I'm a student from the Philippines and I'm greatly in need of your help. I have this job to do to report about the whole process of gold plating but there's are major problem... I don't know the complete process of gold plating and any idea of it whatsoever... and I need to know it very soon - or I'll be dead meat... do you think you could help me with my problem? thanks anyway for taking the time to read my letter and good luck!

MJ BP
- Philippines


March 1, 2009

Hi, MJ. You should see if your school or town library can find some books on this for you:

Gold Plating Technology by Reid & Goldie would be a great one. But you should be able to find a good introductory chapter in most plating texts like the Metal Finishing Guidebook or the Electroplating Engineering Handbook.

Regards,

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.