| Search our quarter-million Q&As |
Home of the finishing HOTLINE since 1989
-----Need titanium Metal foil
Dear Sir, We are searching for the metal foil like Titanium and Aluminum. The gauge is 25 microns to 300. Please help us to find the supplier anywhere in the world. Thanks a lot. Regards,
Jack Huang- Taiwan
1999
Alfa Aesar [A Johnson Matthey Company, Ward Hill, Mass., USA]. I checked their catalog and found titanium foil 0.006 mm thick and larger. -Kirk
Kirk O'Brien- Colorado