Tarnish resistant Silverplate?


(1999)

Dear Sirs

We manufacture Silverplated Tableware and Giftware products made either from Cold Rolled brass sheet or else Sand Casted from Brass scrap. A major problem is with regard to tarnishing of the Silverplate. We would be grateful if someone could provide advice on how to prevent tarnish, at least till the products are on the shop shelves... maybe three to four months, if not longer.

Two parameters are important - the mirror bright shine or colour should not change substantially and the prducts should still be "food safe ".

Thank You

deepak whorra Deepak Whorra
     silver craftwork
New Delhi, India


(1999)

Dear Deepak,

Try 056 from Atotech or if you find it costly use a similar product from Progressive Chemicals Bombay. Both these need to be plated on .

If you prefer to use only immersion type of anti tarnish, GTZ and Chemitall Rai also have excellent products.

Regards,

Khozem Vahaanwala
Khozem Vahaanwala
Saify Ind supporting advertiser
Bangalore, Karnataka, India

saify logo



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.