Eddy Current thickness measurement for Copper Black Oxide?





Can I use an eddy current thickness instrument for black oxide on copper?

Jeff Eckland
- Manteca, California
1999



The lowest standard I have for my PosiTector 2000 is one mil, which is >>much thicker than an oxide coating, so I would say no.

tom pullizzi monitor   tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania
1999


What is the reason for trying to measure the thickness of a copper oxide on copper. This can be done by surface measurements vs. residual after an acid strip of the tube.

Phillip A. Gregg
- Shawnee, Oklahoma
2001




No dead threads! If this page isn't already on the Hotline your Q, A, or Comment will move it there.

Q, A, or Comment on THIS thread -or- Start a NEW Thread



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"