Currently looking to design an outdoor lawn product made of die-cast zinc. We powder coat most of our current zinc parts. With this particular product we need a coating with high corrosion resistance since this part will be used outdoors in the elements. Not familiar with metal coatings since most of our products are plastic. Any idea on what type of coatings can be used for this application would be much appreciated. Thanks.

Mark DiMatteo, product engineer
manufacturing - Somerset, Pennsylvania


(1999)

hi!

you can use e coat it has a very good corrosion resistance.

porat arieh
FURNITURE - ISRAEL


February 27, 2009

Indeed Mr. Porat is correct. IZA tested a number of finishes for zinc die castings a few years ago and found electrocoatings to generally be the best.

Finishing.com has been retained by IZA to update and expand upon this test, and a number of different finishes including electrocoated finishes are in the test cabinet. The best solution may be to electrocoat the parts then powder coat them. Good luck.

Regards,

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.