Electroless plating on silicon wafer


(1999)

hello

My name is Roberto Zepeda from Guadalajara , Mexico.

Now, we have a vacuum deposition process with Al,Ti,Ni,Au,A and Ge .

We are making Thyristors from silicon wafer. My question is how can I get information about electroless plating on silicon wafer to be able to replace our current vacuum process? Now we are exploring feasibility phase to be able to do a analysis benefit-cost to replace this process.

Thank you for your support

Best regards,
Saludos,
Roberto

Roberto Zepeda Delgadillo
semiconductors - Guadalajara, Jalisco, Mexico


(1999)

Electroless nickel plating has been carried out on silicon wafers by several companies for several years. SEMATECH are your best option for more details on the various equipment and processes available.

Kenneth Kelleher
- Ireland



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.