finishing.com -- The Home Page of the Finishing Industry Search our quarter-million Q&As

Home of the finishing HOTLINE since 1989

-----

Chrome-free coating for pretreatment of car bodies?




I am a ChE student at Oregon State University and am doing research on pre-painting coating processes for car bodies. The process is a phosphate conversion coating but my question is regarding the post-treatment: Is there an alternative to using chromic acid in an immersion chrome/water rinse stage? Any advice is greatly appreciated.

Ilanya Strauss
- Corvallis, OR
1999



It sounds as though you have a particular process in mind which uses a chrome rinse after phosphate coating, but I haven't heard of it.

Do you have a specification number you can give to us on-line?

Best wishes,

tom pullizzi monitor   tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania



Hi, Ilanya. If the body is to be electrocoated, and most are, I think it is pretty common to just use DI water as the rinse after phosphate and before e-coat.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
February , 2009


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"