finishing.com -- The Home Page of the Finishing Industry
A website for Serious Education, promoting Aloha,
& the most FUN smiley you can have in metal finishing

HomeFAQsSuggested
Books
Help
Wanteds
Advertise
on this site
FORUM
current topics
topic 3706

Degreasing Method is too expensive


(1999)

Hi

A company that manufactures hydraulic steerings for boats is degreasing the parts from hydraulic oil in a low mp solvent with Ultrasonic and a cooling system.The parts are then spray painted.

The method is successful but the solvent is very expensive. What are the common solvents used?

Are spray jet aqueous systems used in similar applications? Thanks for your help in advance

Mark Camilleri
Malta



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.